I had a partial case head separation using a 1.8oz buffer
Would the brass not get weaker as the walls thin due to stretch and expansion that occurs concurrently during an early unlock, where peak yeild pressure is measurably reduced due to changes in material dimension?

I'm not a mechanical engineer, maybe you can clarify. If there is no failure, then what is considered peak pressure in the formally trained sense as described previously? Just some greater than x equation?